Alec_J
Member
- Joined
- Mar 16, 2017
- Messages
- 89
I balanced my 5 packs of 20p cells to 4.02volts by paralleling them together. All of my cells are new from new replacement laptop batteries and hover board packs. A couple days later one of the packs was at 3.96volts. I thought it was odd at the time but didn't think much more. Yesterday I paralleled the 5 packs again for 14 hours. They all balanced at 4.01volts. This morning I checked and the offending pack was at 3.98 and the other 4 packs were still at 4.01.
So my questions are:
1. is this possibly just voltage sag on this one pack? I am doubtful but thought it worth asking.
2. How do I figure out which cell/cells in the pack are causing the problem?
All ideas welcome
Thanks,
Alec
So my questions are:
1. is this possibly just voltage sag on this one pack? I am doubtful but thought it worth asking.
2. How do I figure out which cell/cells in the pack are causing the problem?
All ideas welcome
Thanks,
Alec